Page 1 of 1

Question to all you JB Weld users

Posted: Mon Oct 11, 2004 10:46 am
by DaMaN
Will it work to patch a small rust inhibited hole in a muffler or exhaust system? If so how long will it last? Is this stuff to be used in small amounts or will it last better if I put on a generous amount?

I think...

Posted: Mon Oct 11, 2004 6:14 pm
by eGoCeNTRoNiX
You'd be better off using some Aluminum tape or muffler tape than you would using JB Weld. Not sure if it will work with the muffler or not.. GL!

eGo

Posted: Mon Oct 11, 2004 6:31 pm
by DaMaN
well the hole is in a crevice so tape = no good

Posted: Mon Oct 11, 2004 9:14 pm
by Pugsley
just get a new one.. they are only like 19 bux unless you got some fancy ass car.

Posted: Mon Oct 11, 2004 9:20 pm
by Lmandrake
I used it to patch a small hole in a tailpipe once and it lasted about two months. But the hole was small and had solid metal all around it. I had some extra from something else I did and just smeared it on. Worked for a while...

Posted: Mon Oct 11, 2004 9:27 pm
by DaMaN
I have holes in the muffler and the Y pipe from the manifold. The Y pipe has a inline built in catalytic converter so it is very expensive. Just want it to last until I can save up the money fop all.

Posted: Mon Oct 11, 2004 9:43 pm
by Ken6PPC
I seriously doubt that JB Weld will last very long that close to the manifold. The pipe will simply get too hot for JB. It releases it's bond at about 400*F, although the web site says it works up to 500*F.

http://www.jbweld.net/coldweld.html

Look on the bottom right-hand side of that site. It says, "Not recommended for use on manifolds, exhaust systems, and other engine components which normally operate at temperatures above 500ยบ F."

I haven't used this epoxy, but it is supposed to be good for higher temperatures. I don't know how well it would fill a hole though.

http://www.hightemperatureadhesives.com ... 20data.pdf